logo
Home News

Casting Defects of Metal Materials, part 8

Certification
Good quality Salt Spray Test Chamber for sales
Good quality Salt Spray Test Chamber for sales
Customer Reviews
Thanks a lot for the professional service of Q1-Test team, we are happy to have the temperature test chamber, and it works well until now.

—— Tonny Cruise

Salt spray test chamber was installed last week according to your guide, it is working well now, thank you. we will recommend it to my friends.

—— Robert Antonio

Our 1000L temperature test chamber QTH-1000C works very well after installed and set by Q1-test service guy. Our staff can operate it fluently. Thanks

—— Juan Smith

I'm Online Chat Now
Company News
Casting Defects of Metal Materials, part 8
Casting Defects of Metal Materials, part 8

 

Casting Defects of Metal Materials, part 8

 

The main defects of casting products are segregation, pores, shrinkage and shrinkage, inclusions, cracks, cold shut and other defects.

 

Other surface defects

Common surface defects of ingots include scars, pitting, pits, burrs, longitudinal streaks, transverse bamboo joints, etc.

 

(1) Roughness

Various unevenness on the surface of ingots is called roughness.

 

There are often granular protrusions and sand holes on the rough surface, accompanied by coatings, covering agents, oxides and other dirt.

 

The main reasons are low casting temperature and slow speed; the inner wall of the crystallizer is not smooth or the covering agent is poor; the funnel is blocked, etc.

 

(2) Burrs

The sharp metal protrusions on the surface, corners, and edges of the ingot are called burrs.

 

The main reasons are the rough inner wall of the crystallizer; the quality of the hollow ingot continuous casting core rod is not good.

 

(3) Longitudinal streaks

The continuous or intermittent longitudinal strip-shaped protrusions or depressions on the surface of the ingot are called longitudinal streaks.

 

The main reasons are that the inner wall of the crystallizer is drilled with metal or other oxides or grooves caused by wear; the inner lining assembly gap is large.

 

(4) Bamboo joints

The large periodic concave and convex phenomena on the surface of the continuous casting billet with a pull-stop process are called bamboo joints.

 

The main reasons are improper pulling and stopping process or deformation of the crystallizer or mold.

 

Pub Time : 2024-08-25 07:57:39 >> News list
Contact Details
DongGuan Q1-Test Equipment Co., Ltd.

Contact Person: Mr. Andy DAI

Tel: +86-13450058229

Fax: 86-769-2278-4276

Send your inquiry directly to us (0 / 3000)